I would suggest trying http://www.rogers-corp.com/ This is the homepage for Rogers Corporation, a fabricator of teflon materials along with other high frequency substrate materials used in PCB fabrication. Westak is one fabricator that I know of whom provides substrates and PCB's with the Rogers 4003 teflon. Hope this helps. Steve Sauer ---------- From: [log in to unmask][SMTP:[log in to unmask]] Sent: Friday, October 16, 1998 9:49 PM To: [log in to unmask] Subject: [TN] Teflon Board Assembly Is there a good source of information available such as white paper or book or articles that explains do's and don't of Teflon board assembly and repair processes. Also, could anyone recommend two to three good Teflon board suppliers. Would appreciate it very much. Please copy me directly on your response at: [log in to unmask] Thanks ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################