Hi Ken: - Although Werner could be correct about the possibility of poor solder interconnect, another thing to consider is that the mass of the component is being restrained during shock test solely by the compliance of the leads and the movement of the component body is exceeding the shear capability of the connection. If you are satisfied that connection integrity is adequate, you might try simply restraining the component body with a dot of adhesive under the component (watch the z-axis CTE of the adhesive). - An obvious, but frequently overlooked, source of trouble could be your shock test fixture and system calibration. Go over the fixture carefully to assure that it is holding the specimen satisfactorily and check the calibration of test instrumentation. - Another question is the type/direction of the applied shock pulse (per TM-650 or some other method?). Is the shock applied to the individual pwa, or to the end item. Seems to me that a half sinewave, 11 ms pulse at 20g peak would be sufficient for qualification testing of most products. I presume that repetitive shock is applied in all 3 primary axis. You might be able to determine which axis is doing the most damage by simply using an optical microscope to examine the specimen after exposure in each axis. Additionally, you might benefit from putting a small tri-axial accelerometer on the specimen and measuring the cross-axis transmissibility ratios during shock to detect any ringing (reflex pulsing or oil-canning) that is taking place. - Guess you have probably already done most of the above, but thought I'd throw in my tupence. Regards, Jim Moffitt ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################