Ed, One more thought on this topic. If this is a multilayer board than its possible that you could have localized heat sinking of the PTH's to an internal power or ground plane. I have seen in the past (via microsections) where the solder flows up the barrel and stops right at the internal plane. If this is the case then its your customers design and or wave parameters that are at fault. Scott >Date: 10-Sep-98 15:03:18 -0600 >From: ED @ SMTP (Ed Cosper) [log in to unmask] >To: TECHNET @ SMTP [log in to unmask] >Subject: [TN] solderability testing > >Hi all, > >Just a quick question. As a board manufacture we typically perform a solderability test ( solder float ) on a small piece cut out of a board that has at least 30 holes. Customers many times will >run a complete bare board thru the wave to check solderability. I have a situation with one customer that I has frequent rejections because one or two holes out of hundreds do not fill during the wave of the bare boards. All of my solder float tests pass >and samples fromt the same lots rejected ran over someone elses wave solder fine. > >I would like to know what most people would accept on that type of solderability test. Specifically regarding instances of when one or two isolated holes fail to fill out of several hundred holes on a 5x8 board. I really do not know if I should expect all > holes to fill 100% without leads. Is there a specific specification that covers wave solder tests on complete bare boards? > >Any help would be appreciated. > >Ed Cosper > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################