I need help tracing the possible root causes for a circuit failure from the field. Does anyone have any experience with open circuit traces due to a silver sulfide corrosion concentrated at the juncture tin-lead solder joints and silver thick films? We are seeing this only on joints that are low voltage potential. There is silver sulfide corrosion at other randomn areas, but the heavy corrosion is primarily at just a few points where the solder and silver meet. Under the microscope, it looks like a black worm crawling along the interface between the solder joint & the silver thick film. We pot the circuit board in silicone gel to protect the circuit from moisture. So far, we haven't traced the source of sulfur to any material that we use to make or to package the circuit board. The packaging does not contain cardboard, so sulfur from the packaging is out. We meticulously clean the board after reflow soldering the printed solder paste, so flux is out. Is it possible that we are getting sulfur gas from the enviroment? The environment is automotive, underhood. Is it possible that there is a galvanic action that is concentrating the corrosion to just a few solder joints? Thank you all for your time. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################