Content-Transfer-Encoding: 7bit We are going to use it for gauging leads. if it is not ESD, then we must use another material. Thanks Paul Stolar ______________________________ Reply Separator _________________________________ Subject: Re: [TN] g10 Author: [log in to unmask]> Chris Chapman <[log in to unmask] at internet Date: 9/17/98 1:53 PM Paul, No! What is your intended use for the G10? Chris Chapman -----Original Message----- From: Paul Stolar <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Date: Thursday, September 17, 1998 2:08 PM Subject: [TN] g10 > Here is a simple question I hope someone can answer for me. > > Is G10 ESD safe? > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################