> Joe, > A few things: > 1) How good a paint do you put on in the first place? > 2) Is it receiving a full cure? > 3) Do you people have enough room to move around in? > 4) Little bottles of the same paint in a Whiteout typewriter correction > fluid bottle can solve a lot of your problems > 5) We use a lot of ESD mats and these also act as very good cushions > > regards, > Bev Christian > Nortel Joe, I'd agree with many of the things Bev suggests. You may get some mileage from using a paint which dries to a harder finish. The paint manufacturers should be able to help you on this. If you have some money to spend, powder coating systems can give very durable finishes with no real drying time. It's possible to put the paint you're spraying (I assume you're spraying) into aerosals. We used to do this and keep some in our packing department to do last minute touch ups. Looking at handling can reduce scrap. Can you change the process flow so the minimum number of handling stages are employed? Making sure all the work surfaces are either foam padded or plastic covered will also help. Good luck, Eric Christison ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################