At a previous employer, I had a line where we reflowed single sided panels (including parts that could not be wave soldered), put the panel on a masking pallet, and wave soldered through hole parts. Yield was very good on both operations, and significantly improved over selective and hand solder. Using an all SMD panel with that design would add a few dollars to a low cost assembly. Pallets were obtained from a standard pallet manufacturer. I have used SPS precision in CA and Midwest Circuit Products in Cleveland. There are a dozen others that I heard can also do good work. Most can also design the pallets for you. ARIC PARR Sr. Manufacturing Engineer Eaton Corp 1400 S. Livernois P. O. Box 5020 Rochester Hills, Mi 48308-5020 [log in to unmask] 248 608 7780 Fax: 248 656 2242 ------------- Original Text From: C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG, on 9/1/98 5:43 PM: To: Aric Parr@01635@Lectron_RH, EatonWHQ@CorpMail@WHQCleveOH[C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG] Hello all, I am looking for feedback on anyones experience in dual mode (SM and TH) manufacturing. We have one SM device, QFP, located in the middle of the PWB with other components surrounding it. We want to reflow the QFP, and then do other placements and then wave solder. We are evaluating masking methods for the QFP in the wave process. I would appreciate any feedback on methods tried, and results experienced. If you have a very positive experience with a specific vendor, I would not mind receiving that info also. I appreciate in advance the response and your time in this. Richard Hamilton Clemar Mfg. / Rain Bird [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################