Joe, A few things: 1) How good a paint do you put on in the first place? 2) Is it receiving a full cure? 3) Do you people have enough room to move around in? 4) Little bottles of the same paint in a Whiteout typewriter correction fluid bottle can solve a lot of your problems 5) We use a lot of ESD mats and these also act as very good cushions regards, Bev Christian Nortel > ---------- > From: Kane, Joseph[SMTP:[log in to unmask]] > Sent: Wednesday, September 09, 1998 5:08 PM > To: [log in to unmask] > Subject: [TN] Paint Finish Protection > > After assembly and test, many of our chassis go back to the paint shop for > touchup of various dings, scuffs, and scratches. We could replace our > clumsy people and buy silk cushions for handling, but are there any other > suggestions? Anyone using adhesive-backed "shelf paper" like you see on > new > cars these days? > > Joe Kane > Lockheed Martin Control Systems > Johnson City, NY > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################