I saw a similar situation with 'D-Pack' devices. The defects appeared totally random, but were related to solder voids at the heat sink tab. What kinds of parts are you seeing this with and what kind of solder paste are you using? >-----Original Message----- >From: Poh Kong Hui [SMTP:[log in to unmask]] >Sent: Tuesday, September 29, 1998 4:30 PM >To: [log in to unmask] >Subject: [TN] Drop off Component > >Hi Technetters, > >I am facing with an issue that the component at the bottom side of >the board drop-off during the second-pass reflow process. However, >such incident happen randonly. > >Could anyone advise me how to resolve such problem ? Thanks > > >Poh > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following >text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section >for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or >847-509-9700 ext.312 >################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################