Our fab vendor refuses to plug any via greater than .015". The most common problem we see with plugged vias is excess height causing screen printing problems. We also see solder balls forming on the top side of the board when the bottom side is reflowed. Our vendor attributes this to the plugged vias. Needless to say we're making every attempt to do away with the plugs whenever possible. > -----Original Message----- > From: [log in to unmask] [SMTP:[log in to unmask]] > Sent: Thursday, September 24, 1998 7:59 PM > To: [log in to unmask] > Subject: [TN] Help! Plugging vias > > > <Original text message attached as document> > << File: ceomail.wrd >> ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################