All, The question was about the interprtation of the allowance to go to 40X to verify a defect seen at 1.75X Measurement oif the size of the defect has nothing to do with the higher magnification allowance. The spec. allows going up to 40X so that the inspector may verify that his defect is really a defect. Often at 1.75X shadows at a nodule, small pits or roughness etc.may appear to be a defect, but when a better viewing at up to 40X is used, it is found to be acceptable. Phil Hinton ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################