In a message dated 8/6/98 8:39:16 AM Pacific Daylight Time, [log in to unmask] writes: << Hello, I am interested in a solution to installing tantalums in reversed. Plus symbols, silk-screen marking, etc. have proven inadequate. Failures come after many hours of reverse polarity in some applications. Are there any ideas on how to physically or otherwise prevent this. Thank you, Rich. >> Hello Rich, Do I sense a bit of frustration? I know where you're coming from, believe you me... I gotta question, are these tantalums machine placed or hand loaded? If they're machine placed, in my opinion it's a little easier to deal with. You've got specific, cut and dried areas to correct and then you're done with it. But if it's hand loaded and you gotta deal with humans, hoo-boy,...that's another story. If you're putting out any kind of assembly aids or some sort of documentation that clearly shows the polarity, and/or the silkscreen is clear, then as much as I hate to say it, it's time to find out who is loading them backwards and suggest they find another line of work. As long as people have been given adequate training, and provided with the proper tools and documentation, there should be no excuse for errors such as that. Those of us that get tasked to correct problems like this on the floor are told a lot of times to do something to make a process or procedure "fool- proof" (a more polite term than what I've heard in the past) in order to be able to hire production workers at minimum wage. Don't get me wrong, I'm not saying that everybody that works for minimum wage is less competent than someone who is getting paid more, but I have heard comments such as this; "Why should I care, I only make five bucks an hour, I'm not getting paid enough to care..." I guess the point I'm trying to make, is that if the problem is coming from hand loaded parts, and you've given them all the documentation they need and/or the PCB is clearly marked, then it's an attitude problem with the people...they don't care enough. You're lucky that the boards only fail...I've been standing next to an ICT station when a board was powered-up with wrong polarity caps...the test technition was extremely lucky that he didn't lose an eye after the caps exploded with enough force to blow holes clean through the PCB... -Steve Gregory- ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################