Werner, Technet people, Would you have any quantitative data about the effect of side fillets comparing to the heel fillet and the "bottom flat" wetting? One of our customers asks us to have a solder fillet up to 50% of the lead thickness on 3 sides of gullwing leads, with a fillet up to the lead thickness (class 3 requirement) on the heel. I was not able to find articles or papers showing the effect of side fillets on the solder joint reliability. I would really appreciate it if anyone could provide me with some information Thanks Emmanuelle Crombez > ---------- > From: Werner Engelmaier[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;[log in to unmask] > Sent: Sunday, August 30, 1998 7:32 AM > To: [log in to unmask] > Subject: Re: [TN] SMT gull wing solder joint force test? > > Hi Mark, > What you are proposing to do is not a good idea. > First, there is no such thing as a standard 'solder joint > force/shear/peel/pull test.' Because of the large variety of solder > joint > geometric variations, there can not be one from this consideration > alone. > Second, the solder joint strength, as determined by a lead shearing > test, has > no bearing on the reliability of the solder joint, provided the test > does not > reveal inadequate wetting. > Third, the fracture surface of the forced solder joints give typically > more > information than do the shear-load histories, because the ONLY really > important finding is whether or not adequate wetting has taken place. > Fourth, the reliability in actual use does to a large extent depend on > the > heel fillet and the 'bottom flat' wetting; if the foot length is <3W, > than > also on the presence of a toe fillet, because short feet 'rock' during > thermal > cycling. Side fillets are less important, unless you have wetting > problems. > Fifth, make sure that your definition of a 'poor' solder joint > corresponds > with ANSI-J-STD-001. > > Werner Engelmaier > Engelmaier Associates, L.C. > Electronic Packaging, Interconnection and Reliability Consulting > 7 Jasmine Run > Ormond Beach, FL 32174 USA > Phone: 904-437-8747, Fax: 904-437-8737 > E-mail: [log in to unmask] > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################