Try methylene chloride to remove the markings; xylene and toulene will also remove some paints. If the parts are laser etched I'm not aware of any chemical that will remove the etching without attacking the package. The package material is a filled novalac resin-the filler is typically 70-90%, depending on where the parts are assembled, and silicon diox is the filler of choice. > ********************************* > Bill Davis, Ph.D. > Diamond Multimedia Systems > Senior Scientist > Tel. 408.325.7868 > Cell. 408.888.5650 > e-mail: [log in to unmask] > ******************************** > > > > -----Original Message----- > From: Edwin Maximo [SMTP:[log in to unmask]] > Sent: Thursday, August 27, 1998 2:20 AM > To: [log in to unmask] > Subject: [TN] ic package > > Hi there! > Can someone tell me what type of material does most IC package are > made of. I've been looking for some ways on how can the top marking > of ICs can be removed or covered. Any inputs will be appreciated. > Thanks in advanced. > > Regards, > Edwin Maximo > Electronic Assemblies Inc. > Philippines > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################