We ran a trial batch of boards using this finish instead of our standard Au/Ni finish employed for mixed and SMT PCBs. Omikron finish would have been around 8% cheaper from our supplier had we swapped over. Results were very good through both SMT and wave solder process, however some solderability problems with subsequent hand soldering operations (we require a few select-on-test resistors to be fitted to each board.) Also minor disadvantage that the inspection benefit from colour contrast between pasted land and unpasted land of Au/Ni finish is lost. Better than HASL for SMT assembly though. Nigel Burtt Production Engineering Manager D - European HQ Email: [log in to unmask] Tel: 01793 842132 Fax: 01793 842101 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################