A good wish list! But you may need to vary attribute parameters of the material to meet the varying needs of your electronic configurations. An encapsulant for a thick small application may not work for a thin large configuration. Increasing the filler loading, type of chemistry (e.g., biphenyl vs multifunctional, etc), sophistication level of your supplier and volumes you buy will decide most of the parameters you have listed. Some of the parameters like voids may very well be a function of your process. Syed. -----Original Message----- From: Edward Boucher [SMTP:[log in to unmask]] Sent: Wednesday, August 12, 1998 2:49 PM To: [log in to unmask] Subject: [TN] The ideal eletronic encapsulation material? Greetings Technet, Dose anyone know of a encapsulating material for electronics, which can meet the majority of these parameters? We have been searching for about a year and have had little success. The Ideal Encapsulation Material a. low toxicity b. low moisture permeability c. no or very low ionic content d. low viscosity e. low linear shrinkage f. low glass transition temperature (Tg) g. low Coefficient Of Expansion (CTE) h. low embedment stress i. high tensile strength j. high thermal conductivity k. void free l. electrical insulation properties m. thermal cycling stability n. high thermal shock resistance o. wide temperature range -55 to 95 degrees C p. good chemical and solvent resistance q. good adhesion r. low cost s. ease of processing (application and clean up) t. no formation of water u. non-corrosive v. easily repairable Your help is appreciated... Ed Boucher Engineering R&D Tech. K and M Electronics 413-263-6253 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################