Inform your customer that a contract for soldering to MIL-STD 2000 is uninforceable. The closing of the Goverment Schools rendered MIL-STD 2000 Task G impossible to achieve. There is no Category certification available to meet the requirements of the specification. Are they calling out MIL-STD 2000A whose requirements can be met? They are actually very different documents and have different lead tinning requirements. Single point soldering is soldering one termination at a time. I will fax you Mil-STD 2000 Par. 4.11.3 , par. 5.4.4, and par 5.4.17.6 Al Cash > ---------- > From: Rick Thompson[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;Rick Thompson > Sent: Thursday, August 27, 1998 4:43 PM > To: [log in to unmask] > Subject: [TN] MIL-2000 Lead Tinning? > > Hi, > > We have a customer who is requesting a quote to build PCBAs with a > requirement for lead tinning & 'single-point' soldering per Mil-2000. He > knows that Mil-2000 has been superceded but their customer is still > requiring it. I don't have a copy of Mil-2000 and was wondering if > someone > could briefly tell me what the lead tinning requirements of the spec were, > was it a requirement at all times or only when solderability testing > failed, > etc. Also, what the term 'single-point' soldering refers to; I'm not > familiar with the term. > > Thanks. > > Rick Thompson > Ventura Electronics Assembly > 2665A Park Center Dr. > Simi Valley, CA 93065 > > [log in to unmask] > > (805) 584-9858 voice > (805) 584-1529 fax > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################