Bruce - I would recommend you go very cautiously with any type of underfill material. This poses a TCE differential situation, which could result in solder fatigue. Most electronic products end up with some degree of thermal cycling, whether from power on/off or their operating environment. The TCE of solder is relatively low in comparison to most plastic materials, therein lies the risk of a stress situation. If your operating temperature range takes you above the glass transition temperature of the material, this will further increase its expansion coefficient. Lastly, if your operating temperature takes you into the -40C or below range, most of these materials will go almost rock hard, which may give you another factor to reckon with. If this is an absolute "must do" situation, some of the silicon gels or dead soft urethanes might be candidates for equipment operating in a very benign environment. A dipped conformal coating might also serve the purpose of coating the conductive surfaces, without full embedment of the area under the part. Parylene also works very well for this type task. Good luck - Kelly ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################