Clive, S stands for Silica. The filaments are pure silicon dioxide which has a much higher melting point than E-glass. There is almost no sale for the stuff which is very expensive and I am told is a real pain to process. You have to really really want it to go to this much trouble. You can get lower dielectric constant materials from ourselves and others. Regards David Heywood. -----Original Message----- From: [log in to unmask] Sent: 26 August 1998 17:15 To: [log in to unmask]; Dave Heywood Subject: [TN] DES: "S-glass" Fibre Reinforcement << File: ENVELOPE.TXT >> -------------------------------------------------------------------------- -- Hi All, Does anyone out there have any information or specification details on "S-glass" fibre reinforcement material as used in PCB laminates, and what does the "S" stand for? There are TCE (sorry CTE for you guys!) advantages with its use, and depending on the resin system it is used with, Er advantages also, but I am looking specifically to identify and understand the differences between "S-glass" fibre material and the more conventional "E-glass" fibre material. (I understand "E" stands for "Electronics" Grade???). How many people use S-glass? What benefits do you see? Any comments appreciated. Clive ffitch Matra BAe Dynamics UK Stevenage, England E-mail [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################