Ron, Check out Metcal's website @ www.metcal.com, they have a wealth of information on their systems. One of the great features for an ISO operation is the fact that calibration is never required, it's worth the price for that even without the superior performance they provide. We have over 150 units here, and would never switch to anything else.... Mike McMonagle PCA Process Supervisor K*Tec Electronics (281) 243-5639 > -----Original Message----- > From: Ron Hollandsworth [SMTP:[log in to unmask]] > Sent: Friday, August 14, 1998 7:15 AM > To: [log in to unmask] > Subject: [TN] MetCal Irons > > We are using a no-clean handsoldering flux. I have seen and > heard > many stories of how good MetCal irons are for a no-clean > operation. > Maybe I could get some listners here to take note of the > importance of > iron temperature and no-clean if you TechNet buddies out in the > World > would drop a line or two onto the TechNet about the pros and cons > of > the MetCal soldering irons. Perhaps I may be able to convince > others > in this organization that this is the way to go for tip > temperature > control. > > I would appreciate the help. > > Thanks > Ron Hollandsworth > Operations Task Leader > Advanced Manufacturing Engineering > [log in to unmask] > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################