Jeff My opinion would be that as long as your auto-insert machine isn't hitting the parts with the clinch mechanism you should be OK in that machine - check the clearances. However, consider that the boards will see a lot more handling, and you will likely have a lot of missing parts from boards being banged. Ensuring good handling procedures and a good process flow will be essential. regards, Graham Collins Process Engineer Litton Systems Canada (902) 873-2000 extension 215 -----Original Message----- From: Jeff Hempton [mailto:[log in to unmask]] Sent: Monday, August 03, 1998 12:43 PM To: [log in to unmask] Subject: [TN] stencil printing bottomside glue Good morning Technetters! Hopefully I have given everyone enough time to ingest their favorite form of artificial adrenaline (AKA caffeine) to get you moving on a Monday morning. I could use your expertise for the following concern: I searched thru the archives but could not find direct info on this: I am crunching numbers for a high-throughput bottomside (glue-n'-chips, then wave) product, and in order to meet the rate required, I am considering stenciling glue instead of dot-dispensing. The concern is that I have a few auto-insert radial components (not available in SMD) that then must be inserted AFTER the glue stencil operation. My question: 1) Should I be concerned about the forces of radial auto-insertion and clinch causing problems with my glued-but-unsoldered chips? 2) If someone has already been thru this, is there anything special you had to do (tooling, prayers) to insure chips were not flying in all directions? What were your success/failures? Any feedback would be greatly appreciated. Jeff Hempton United Technology Electronic Controls ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################