Howard, My understanding of Pacovia is that it's designed to flow under pressure even at low temperature. This is supposed to allow it to perform a damming function around openings before the resin flows. However that characteristic implies that it may not do well with too much heat and pressure. I'd have to go find the data sheets to know if you're exceeding its' capabilities, but what are your lamination parameters? Time, Temp., Pressure, and Heating Rate. (The heating rate has a significant effect on minimum viscosity and flow.) What's the whole stack-up layering? While I've found the PACO products to be pricey, they are typically of the highest quality and work as designed with a reasonable amount of room for process development. Andy Magee Flex Guru [log in to unmask] Howard wrote, I got some troubles on sequential lamination for blind vias. Because the resin will flow onto the copper surface during lamination process, it will get troubles on pattern forming process. I use PACO VIA #4000 for release film on lamination process. But I found there are two issues that I should care. One is the cost of PACO VIA very high, the other is that there is some residual on seperate plate after lamination process. Is there any recommend for sequential lamination process? I wish I can get solution from you as soon as possible. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################