Tom, Try visiting the www.norplex,com and you should be able to get the information. Norplex's NP424 is a UL approved CEM-1 material with flammability rating of 94V-0. K.K. Chin Mfg Engg Manager Artesyn Technologies www.artesyn.com From: Tom Burek <[log in to unmask]> AT NetMail on 07/20/98 05:32 PM EDT To: [log in to unmask] AT NetMail@ccmail2 cc: (bcc: KK Chin/NA/Artesyn) Subject: [TN] CEM-1