---------- > From: Michael D. Doty <[log in to unmask]> > To: [log in to unmask] > Subject: [TN] Dump Criteria for Solder Strip > Date: Wednesday, July 01, 1998 10:21 PM > > > I'm looking for dump criteria on solder strip in a Tab line. I > currently dump on board count but would like to know if 1.) There is a > copper concentration I could dump to or 2.) it is overkill? > I can't seem to get any info on this from vendors or other users. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ Michael, Look in Manko's book, I believe he gives a figure. Frank Komitsky, Jr. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################