Does the 10 mil spec correspond to a ball size? What about a microBGA with a 5 mil ball size? Thanks. Syed. -----Original Message----- From: Ken Patel [SMTP:[log in to unmask]] Sent: Friday, July 10, 1998 4:22 PM To: [log in to unmask] Subject: [TN] Provide me your current BGA Spec on void Technetters, What is your current spec on accepting void in BGA joints? Are you going by spec of 10 mil, meaning void more than 10 mils is reject? What are your customers specifying in assembly drawings? re, ken patel ______________________________________________________ Ken Patel Phone: (408) 490-6804 1708 McCarthy Blvd. Fax: (408) 490-6859 Milpitas, CA 95035 Beeper: (888) 769-1808 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################