We have done some reliability testing on Ni plated vias. The affects and impacts of the Ni plating depend highly upon the thickness and continuity of the Ni plating. In summary, Thicker layers of Ni, which are free of voids with the high Tg resin system we use, show that the ability of the pth to withstand thermal stresses increases. Also, corrosion concerns go away. The area of concern is getting that perfect Ni coating. Many electroplate processes do not have enough throwing power to deposit enough Ni in the hole. Also, if you get a bubble void in the Ni, the stress of thermal expansion is concentrated in a smaller region of the Cu, making failure occur much sooner. Given different intentional Ni thickness' we have been able to double the life of the Cu pth, or half it. A bubble void in the Ni can bring it to nearly 0. So, the key variables that need to be addressed include; - Plating thickness - Particular Resin and its Z expansion - Plating quality (freedom from thin spots, voids, etc. My personal recommendation is that if you have high aspect ration product (>7:1), unless you have exceptional process control, you may not want to try Ni. For thin product it works fine. The telecommunications industry is practically all Ni/Au as a surface finish on such boards as cell phone boards. These low aspect ration products are less prone to the thickness and voiding concerns. Jim Herard KBL, Product Quality Engineering IBM Microelectronics Endicott t/l 857-7026 referenced note: ------------------------------ Date: Wed, 8 Jul 1998 11:59:43 -0600 From: "Signorelli, Paul" <[log in to unmask]> Subject: Nickel Plated Via's Has any one seen any reliability data for Nickel/Gold Plated Via's ? This process is used to prevent copper corrosion from 'air bubble' plating defects, plating residues and from flux residues after assembly. Paul Signorelli Reliability Engineer RW Systems Fax 719-3822520 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################