PTFE is a thermoplastic. At soldering temperatures, the peel strength is ZERO. Rogers has an applications note measuring copper peel strength vs. temperature that will confirm this. For hand assembly, controlled temperature soldering irons should be used. You have to keep an eye on the operators because the like to turn the temperature up so that their work goes faster. Secondly, the solder or solder wick should be removed from the work before the soldering iron. Most operators think they remove them both at the same time, but in reality one comes off a fraction of a second before the other. As soon as the heat source is removed, the solder begins to solidify. The dielecric has a very low thermal conductivity and is slow to cool down. The peel strength is still zero and it takes very little to lift lines. Let me know if I can be of any further assistance. Ron Desilets Sales and Marketing Manager Graphic Research, Inc. 818/886-7340 > ---------- > From: Jan Satterfield[SMTP:[log in to unmask]] > Reply To: TechNet E-Mail Forum.;[log in to unmask] > Sent: Tuesday, July 14, 1998 10:24 AM > To: [log in to unmask] > Subject: [TN] ASSY: Duroid Material > > > > We assemble many SMT boards made of Rogers Duroid. Our problem is > with > traces and parts of terminal pads coming off during the hand > soldering/hand cleaning operations. I have read through the TechNet > archives and Rogers home page and have found nothing addressing this. > We are using a RMA flux and hand cleaning with IPA (occasionally MEK). > I've also noticed that some of our boards come from the vendor with > what > looks like mouse bites out of the pads, and this is before we have > soldered anything to the board. > > Has anyone else had this problem and what have you done about it. All > suggestions appreciated. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################