try Epoxy Technology (508-667-3805) >>> Brent Alcorn <[log in to unmask]> July 22, 1998 6:17 am >>> Percy Childe wrote: > > Can any one help me to get a list of suppliers of condutive expoxy > adhesive? > Can any one give me the web address of W.R. Grace & Co. Alpha Metals > Inc and > Armicon? > > Best Regards Percy Childe One company of conductive expoxy is LOCTITE : www.loctite.com Possibly Dow Corning, Litton ? For Apha Metals Inc try: http://ns.alphametals.com/index.html Regards, Brent J.J. MacKay Canada Ltd. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################