Two years back I investigated use of DBT foil with a reflective system AOI (Orbot 1132 unit). Our core laminate supplier used 2 or 3 foil vendors which varied greatly in appearance from orange - copper colored to olive green. We were able to set up the AOI to easily run the orange colored copper DBT foil but not olive green foil...as you said not enough contrast between laminate and foil. We recently purchased a 1411 reflective AOI unit and were informed it would be capable of inspecting DBT foil only if the foil treatment was highly consistent. We have not tried running DBT yet and have no info. with this new AOI unit. The contact @ Orbotech that I worked w/ on this matter was Dave Fisher. 978/901-5182 Phil Dam ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################