Pac Tech, Am Schlangenhorst 15-17, D-14641 Nauen, Germany Ph 49 0 30 467 815 71 Fax 49 0 30 467 815 27 Contact Elke Zakel, Dr.-Ing., General Manager, [log in to unmask] -----Original Message----- From: Kathy Palumbo [SMTP:[log in to unmask]] Sent: Friday, July 17, 1998 12:23 PM To: [log in to unmask] Subject: [TN] BGA Ball Attachment Process I need to attach BGA balls to a PCB. Does anyone out there know how this Balling process should be done? Is there anyone out there capable of performing this Balling Process for me, or can you recommend equipment that could do it for me? Your help in this matter is greatly appreciated!! Thanks in advance!! Sincerely, Kathy Palumbo ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################