u could use solder balls that are available in the market and place them by hand using pincers with the balls dipped in flux, which are then reflowed. we do these at our lab for shear testing purposes. though a bit cumbersome, the results are good PARVEZ M.S. PATEL ADDRESS: GRADUATE STUDENT, APT.#2, 22 FLORAL AVENUE, SYSTEMS SCIENCE AND INDUSTRIAL ENGG. BINGHAMTON, NY-13905 STATE UNIVERSITY OF NEW YORK, NEW YORK. U.S.A. BINGHAMTON-NY. PH:607-770-7507 EMAIL:[log in to unmask] [log in to unmask] URL:bingweb.binghamton.edu/~bg22842 On Fri, 17 Jul 1998, Kathy Palumbo wrote: > I need to attach BGA balls to a PCB. Does anyone out there know how this > Balling process should be done? > > Is there anyone out there capable of performing this Balling Process for me, > or can you recommend equipment that could do it for me? > > Your help in this matter is greatly appreciated!! > > Thanks in advance!! > > Sincerely, > Kathy Palumbo > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################