The melting point of pure Nickel is 1453 deg C, the Boiling Point is 2730 degrees C. ---------- >>>From: Ruben Irizarry >>>To: [log in to unmask] >>>Subject: [TN] Nickel Melting Point >>>Date: Thursday, July 16, 1998 8:31AM >>> >>>I am in a rush and need thwe melting point of pure Ni. Will someone help >>>me? >>>Thanks in advance >>>Ruben >>> >>>################################################################ >>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >>>################################################################ >>>To subscribe/unsubscribe, send a message to [log in to unmask] >>>with following text in the body: >>>To subscribe: SUBSCRIBE TechNet <your full name> >>>To unsubscribe: SIGNOFF TechNet >>>################################################################ >>>Please visit IPC's web site (http://www.ipc.org) "On-Line >>>Services" section for additional information. >>>For technical support contact Hugo Scaramuzza at >>>[log in to unmask] or 847-509-9700 ext.312 >>>################################################################ >>> >>> ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################