Hello KK Although I'm not 100% sure, I believe the Laminate data convention is the X is the warp (i.e. grain or machine direction of the treated fabric) and the Y is the fill (i.e. weft or cross grain direction of the treated fabric). If you know the lay-up construction detail, you will know which is which. Most board shops specify grain orientation for their laminates and prepregs. Most board shops would be happy to tell you. If it is not known, the only way I know to determine the fabric warp direction, assuming the lay-up does not cross-ply prepregs, is to burn the resin & copper layers off in a vacuum furnace. This should leave the glass fabric layers only. Using a "linen tester" you would then count the number of threads per inch in both sample directions. You would then compare the numbers to a fabric chart (either IPC spec or glass fabric vendors can provide) which will tell you the thread count in warp and fill directions. Hope this helps. Gerry -----Original Message----- From: KK Chin [mailto:[log in to unmask]] Sent: Tuesday, July 14, 1998 7:29 PM To: [log in to unmask] Subject: [TN] CTE of PCB Laminates Specs from laminate manufacturers show a substantial difference in coefficient of thermal expansion between X-axis and Y-axis for FR4, FR2, CEM3, CEM1, etc. Is there any way I can tell from a finished PCB which is X and which is Y? How can I specify in my PCB drawing such that a fab. house always orientates my PCB in a particular axis? I consider this as a mean to match with the CTE of certain components on that PCB. Thanks! K.K.Chin ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################