With increased layer count and ground plane shielding requirements we are having trouble obtaining the 75% vertical fill requirement(IPC J-STD-001B) for through-hole leads. A typical application is a 16 layer polyimid board about .120 thick. This board has one ground plan and several sectional voltage planes. The board will be part of a GPS satellite system with a 15 year mission. We will install 15, 220 pin through-hole motherboard connectors on the board. Our boards are fabricated in lots of two or three. In the past all our soldering was done by hand and we required 100% vertical solder penetration from the source side to the destination side. As our boards have become thicker we went to wave soldering to get proper penetration. Now with thicker boards that is not always a reliable method. More I/O requirements have pushed us to four row connectors making it impossible to inspect on the inside pins anyway. With current printed circuit board manufacturing techniques I am wondering if barrel reliability is good enough to only command good wetting on the source side and let the penetration be what it will. I think all of industry has stopped putting "Z" wires in unused vias to ensure barrel reliability. Can I stop using the connector pin for the same reason? Are there other issues to be concerned with? I am interested in any data or testing someone has done or just plain opinions. Thank you Jim Payne, Sandia National Labs (505) 844-3336 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################