Frank- I have some DuPont literature that says..."Nonwoven aramid reinforced laminate is typically supplied at 50% resin content, by weight, to meet the needs of low in-plane CTE applications (8-10 ppm/C). By varying resin and copper content in final boards, CTE can be tailored to any design point between (8-16 ppm/C)." DuPont calls the nonwoven aramid reinforcement "Thermount", which is a DuPont registered trademark. In looking for additional aramid info, I found that the terms Aramid, Thermount, and Kevlar might be used interchangeably, and finding the chemical origin of aramid wasn't an easy task. On this note, the following references clarify the names and polymer system information: 1) "...aramid (aromatic polyamide polymer) fibers...have been developed over the last 20 years" 2) "The aramid fiber is manufactured by E. I. DuPont de Nemours & Co. under the trade name Kevlar. IPC-A-142 documents the specifications for finished fabrics woven from aramid material." Excerpt 1) is taken from pg.2.13, and 2) is taken from pg.2.14, respectively, of "Electronic Materials & Processes Handbook", Eds. Charles Harper and Ronald Sampson, 2nd Ed., McGraw-Hill, ISBN 0-07-054299-6, (1993). Table 2.1, pg. 2.14 of the same text lists the CTE of Aramid fiber as -5.0 ppm/deg C (along the fiber axis; radial CTE = +60 ppm/deg C). Note that the axial CTE is a negative number! -Michael Alderete +++++++++++++++++++++++++++++++++++++++++++ +++++++++++++++++++++++++++++++++++++++++++ You wrote... ------------------------------ Date: Thu, 23 Jul 1998 13:30:12 +0000 From: "Frank K. Frimpong" <[log in to unmask]> Subject: CTE of PCB material. Hi Techie persons, I need some help on this. 1. Carbon fibre has a negative CTE. The result of combining it with a high positive CTE resin such as epoxy is a composite with a good dimensional stability. Can any one tell me if Aramid fibres also posess a negative CTE and if so what is it? 2. Various constraining layers can be introduced within PCB's in order to improve the thermomechanical properties. One such system is the introduction of a copper-invar-copper layer. Can anyone point me towards some published articles or manufacurers of this system or other similar systems. I would also like to know at what stage of the manufacturing process is the system introduced, and what effect does it have on the cost, performance and reliability of the assembly. Thank you. ------------------------------ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################