Is there anybody having experience on Wave Soldering Ceramic Capacitors C2225C225M5UAC ? We are using these caps on solderside of one of assembly (Gluing the Components ) .We are finding some of caps blowing off at ATE. Our manuf engr is suspecting wave thermal shock /mech shock? KEMET has in one of their application notes mentioned that this part should not be used for wave soldering. Special process profiles required. Any recommendation for our wave soldering Process Engineer? I will appreciate if somebody can share experience on Technet and provide info. thanks Ashok Dhawan P.ENG. Manufacturing Engineering Unisys Canada Inc. 51 Burmac Road Winnipeg R2J4C9 CANADA Fone 204-257-9199 Fax 204-257-9104 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################