Sorry to inform you that the manufacturer discontinued this product more than a year ago due to very low volumes. Bob Stumpf >>> Lisa Parker <[log in to unmask]> 07/17/98 08:03am >>> We used to buy a diazo adhesive transfer film from Glenbrook Technologies (P/N IP2-LIT-MAT size 8.5x11, 2 mil clear, sepia standard speed, Imtac). This is no longer available from Glenbrook, Rexam, GMP, Morton. Apparently no one manufactures this film any more. If you have some of this film (brand or size is not important) I would like to buy some. Do you have any suggestions as to what to use instead of this. (We use it for date codes on artwork.) Lisa Parker, Purchasing Agent ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################