Ed, If the minor chemical constituents in the CFC based cleaners didn't foul you up, then n-propyl bromide won't. regards, Bev Christian Nortel PS Not all n-propyl bromides are the same purity, but this statement is not meant as a reflection on the supplier you mentioned. > ---------- > From: Edward Boucher[SMTP:[log in to unmask]] > Sent: Wednesday, July 15, 1998 4:05 PM > To: [log in to unmask] > Subject: [TN] N-Proply-Bromide (Ensolv) compatability with Uralane > 5753 and 5750 > > Greetings Technet, > > In 1992 we had a aerospace application where we required the use of > Uralane 5753 (conformal coating) and Uralane 5750 (potting). The Uralane > Mfg. is Ciba Specialty Chemicals. At that time > portions of our cleaning process called for the use of Genesolve and Freon > (TMS). Our concern is whether or not there are cure inhibitions or > adhesion problems when using N-Proply-Bromide(Ensolv) with Uralane 5753 > and > 5750 in standard electronic manufacturing processes. > > Please advise with any pertinent information or direction. > > Thank you Ed Boucher > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" > section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################