In a message dated 6/10/98 11:19:30 AM Pacific Daylight Time, [log in to unmask] writes: --> To all, --> --> My R packs have a mind of there own, at pick and place they are aligned --> then during reflow they decided to move. What causes this and how can I --> prevent this? --> --> Thank you in advance --> Angie Hi Angie! I'm assuming you're talking about chip resistor networks, because I know there can be a problem with them if you have a certain style termination. There's quite a few people not aware that there ARE two different styled terminations; Concave and Convex, or as I prefer to call them; "Innies" and "Outies"...ya' know, like belly buttons (GRIN). To describe them a little further, is that Concave styled terminations are also known as castellated terminations, or what you see on LCCC's (Leadless Ceramic Chip Carriers), there will be a square shaped metallization with a half circle shape on the face of each resistor on the network. The Convex terminations have the metallization plated all around the end of each resistor looking more like the standard termination on individual resistors. The best ones to use are the "Innies" or concave terminations. They don't have the skewing or misalignment problems that the convex terminated networks have. The "innies", because of the termination design, utilize the surface tension and wetting forces occuring when the solder is liquidous to a much better degree than do the "outties" and actually self-center during reflow. In fact, I have a report that was given to me by a Phillips component rep, of a study done by engineers in the Phillips product application group to quantify that there really is a difference between the two styles. It has some really nice pictures of the two styles before reflow, and after reflow. They've both were placed misaligned to the same degree, and the pictures show that the "innies" self-aligned while the "outties" did not. Unfortunately, I only have a hard copy of this report, and it's in color so it doesn't copy clearly in a black and white copier, otherwise I could FAX you a copy. I don't have a scanner, but I do have a digital camera, so I'll try and take a clear picture of the one page of the report that shows the before and after pictures clearly and email them to you if you want... But, I bet you that's your problem...I went through the same headaches when I first started placing them. We we're building SIMM cache' modules that had 16-per of these little jewels on a board. -Steve Gregory- ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################