Brett, There is some of your processing info missing that would help give you a better answer. 1) Do you clean, and with what, after the hybrids are reflowed the first time? 2) Are you printing a thickfilm conductor or is this a thinfilm solderable on ceramic. What type of conductor is it (i.e., Pt/Ag, Pt/Pd/Ag, etc??)? 3) What thickness is your ceramic? 4) Have you profiled?? Those ceramics soak a heck of a lot of heat, ya know. I have had some similar problems with a Pt/Pd/Au thickfilm conductor that was printed over dielectric. The material was sensitive to shelf life, since the platinum seemed to "oxidize" somewhat, but N2 storage helped. Also, I remember having similar problems when we were co-firing thickfilm dielectrics and solderable conductors...the material that was burning off the dielectric during firing was detrimental to the solderability of the conductor. Again, more process info could probably provide some better answers. Good Luck. Jeff Hempton United Technologies Electronic Controls ______________________________ Forward Header __________________________________ Subject: [TN] Pinholes in reflowed SMT Author: Brett Goldstein <[log in to unmask]> at Internet Date: 6/26/98 9:51 AM I wonder if anyone out there can help me with this problem. We've been observing multiple pinholes in the solder joints of SMT components (0603 and 0805 resistors and caps) that were reflowed in a batch reflow oven. These parts are being reflowed on ceramic hybrids. The process flow is to print solder paste on the hybrids, reflow the solder paste, apply some paste flux, place the components, and then reflow the hybrids again. (We use this process because we may manufacture 100 or so of the ceramic substrates at once, but then place components on only a few per day.) Any idea why we getting these pinholes? Thanks for your help. Brett Goldstein EVI, Inc. ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################