Dave Pick -"process engineer" wrote: > > I am looking for a temporary way to mark defects on a PCB assembly (other than > the red arrows that everyone uses). The boards will go back through a water > wash, so I was thinking a water soluable, non-conductive ink would be nice. Are > there any recommendations? > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ Dave - Try contacting Metron Optics in Solana Beach, CA for marking pens that have both removable and permanent fluorescent amrking inks. Telephone: (619) 755-4477, Fax: (619) 755-4752 Ed Valentine/ -- ProTronics, Inc. 861 Old Knight Road Knightdale, NC 27545 Phone: (919) 217-0007, Fax: (919) 217-0050 http://www.protronics-inc.com ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################