Make sure you are using good entry material (preferably aluminum). Rout Lead wrote: > SOME POSSIBLE CAUSES ARE SPINDLE RPM AND IN FEEDS, ALSO YOUR PANEL > STACK HEIGHT.THESE ARE THE THREE FACTORS THAT YOU NEED TO LOOK AT WHEN > USING A SMALL DRILL BIT LIKE AN .0240 IF YOU ARE DRILLING THREE DEEP > TRY USING A SLOWER FEED RATE AND A HIGHER RPM. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################