Thank you for the responses we've received to our question on ultrasonic cleaning. However, the question was worded poorly and also did not cover the topics we wanted it to. So we're going to give it a second go. Lately, we have experienced some problems with gold to nickel adhesion. We are using nickel/gold plating as an etch resist for an ammoniacal etcher. The parts have a dry film image placed on them prior to plating. Immediately following nickel/gold plating, the parts are tape tested. They are then sent to have the dry film removed and then etched. Following the etching process they are again tape tested. Occasionally, the first tape test will produce gold peeling, and the job gets reworked then. Most of the time, however, the gold holds up through the first tape test, and most adhesion problems that we have don't show up until after etching. It also seems to happen more frequently on TMM material then on others. Any suggestions you may have would be a great help to us. Thank you Ryan Modular Components National, Inc. 2302 Industry Court Forest Hill, MD 2150 PH (410) 879-6553 Fax (410) 838-7629 ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################