What formula do you wish? Chemical reaction & material consumption can be found in an article in Plating and Surface Finishing, October 1981 by Richard E. Horn. If you would like, I could fax it. George Carroll, Process Chemist [log in to unmask] (804)978-5419 -----Original Message----- From: Steven R. Page [SMTP:[log in to unmask]] Sent: Monday, June 01, 1998 3:53 PM To: [log in to unmask] Subject: [TN] help!! Hello and good day, I am in need of the formula used in electroless plating. I was hoping you could help me. I have been searching the net for over two weeks now with no luck. I know someone out there has this information. I just don't know where to look obviously. :-) I will be waiting for your reply. Sincerely, Cathie Smith ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################