Bill, Write little bit more about your process ( vertical , horizontal , surface preparation , process control , etc ) regards At 07:57 15/06/98 -0700, you wrote: >Yo techies! Has anyone out there had experience with Ethone-OMI's Enteck OSP? We're using it here as we have some 0.4mm pitch devices & have had problems managing the thickness of the OSP. We see residues which causes non-weeting on the pads, & the gold edge connector still had enough OSP left to cause connection problems. Any help would be greatly appreciated... > >################################################################ >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c >################################################################ >To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: >To subscribe: SUBSCRIBE TechNet <your full name> >To unsubscribe: SIGNOFF TechNet >################################################################ >Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. >For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 >################################################################ > > Edward Szpruch Eltek Ltd - Israel Tel 972 3 9395050 Fax 972 3 9309581 E-mail : [log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################