Ernst, >From a manufacturing stand point, space around the BGAs are needed to facilitate rework. Without the space, components around the BGAs will be damaged during rework. Your manufacturer will charge heftier price to manufacture those boards without the space and in worse case you may have to scrap the boards that require BGA rework. _____________________________________________________________________ You don't need to buy Internet access to use free Internet e-mail. Get completely free e-mail from Juno at http://www.juno.com Or call Juno at (800) 654-JUNO [654-5866] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################