How about excluding oxygen and moisture? ---------- From: Stefan Pollmeier[SMTP:[log in to unmask]] Reply To: TechNet E-Mail Forum.;Stefan Pollmeier Sent: Thursday, June 04, 1998 12:29 PM To: [log in to unmask] Subject: [TN] Reflow soldering: forced gas vs. infra-red Dear TechNetters, a contract manufacturer has problems in controlling the soldering process after switching to forced gas (from infra-red). One idea was letting us change land patterns ("my experience: oval works better than rectangular"). Any experience reports, hints, literature regarding land patterns _and_ soldering process would be welcome. Any hints on process optimization we could forward to our contract manufacturer are also welcome (is there a "top ten faults in forced gas convection soldering"?). Thank you very much in advance. Best regards Stefan Pollmeier -- Stefan Pollmeier [log in to unmask] ESR Pollmeier GmbH Tel. +49 6167 9306-0 Lindenstr. 20 Fax +49 6167 9306-77 D-64372 Ober-Ramstadt, Germany ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################