Duane, We ran into the same problem about two years ago. We were having to clean the boards with acetone to get the residue off, not to mention the time for actually masking and unmasking the boards. We now use Spot Mask, a liquid latex rubber compound from Weller. It goes on pretty fast. We air dry the boards, although sometimes when we are in a pinch, we use the oven from an old Amistar P&P machine at 347 degF and 3.5F/M. Unmasking is a breaze. Just peel. Hope this helps. Jared Lang Manufacturing Engineer Minarik Corp. > ---------- > From: Duane Briggs[SMTP:[log in to unmask]] > Reply To: [log in to unmask] > Sent: Monday, June 01, 1998 11:29 AM > To: [log in to unmask] > Subject: [TN] Tape residue elimination > > Gold fingers have to be covered during flow soldering. Is there any > tape > that does NOT leave ANY residue? If not, what is the best, cheapest > way of > removing the residue? Pallets are not an option for us unfortunately. > > Duane > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV > 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################