LPI Richard Blanchet Process Engineer, screening Viasystems Canada Inc. tel.: (514) 694-8900, ext. 4189 fax: (514) 694-9776 [log in to unmask] > -----Original Message----- > From: Afri Singh [SMTP:[log in to unmask]] > Sent: 23 juin, 1998 18:49 > To: TechNet E-Mail Forum.; Blanchet, Richard > Subject: Re: [TN] Fab: plug vias > > Is this thermal,UV or LPI ink ? > > On Tue, 23 Jun 1998, Blanchet, Richard wrote: > > > Hello, > > > > If the solder mask in the vias has been cured (full plug), is there > any > > way to remove it without damaging the boards ? There's no solder > mask > > on the surface beside in the vias. Thanks. > > > > > > Richard Blanchet > > Process Engineer, screening > > Viasystems Canada Inc. > > tel.: (514) 694-8900, ext. 4189 > > fax: (514) 694-9776 > > [log in to unmask] > > > > ################################################################ > > TechNet E-Mail Forum provided as a free service by IPC using > LISTSERV 1.8c > > ################################################################ > > To subscribe/unsubscribe, send a message to [log in to unmask] with > following text in the body: > > To subscribe: SUBSCRIBE TechNet <your full name> > > To unsubscribe: SIGNOFF TechNet > > ################################################################ > > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for > additional information. > > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > > ################################################################ > > > > ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################