I am trying to determine the differences between Probimer-52 and other soldermasks (Tamura, Taiyo, etc.). I understand that application techniques differ, as Probimer requires a curtain coating process, while the others can be sprayed, etc. Are there significant differences between Probimer-52 and others? If so, what are they? Is one better then the other? I am trying to make an argument for the changing to a more conventional S/M and any feedback would be greatly appreciated. Thanks for all of your help in advance. Best Regards ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################